Wednesday, January 5, 2011

submerged arc furnace

Metallurgy of metal and non-metal for silicon, alloy iron, zinc, calcium-carbide, matter, phosphor, phosphonium boron and so on

Model
Smelting steel grade
Rated capacity
(KVA)
Hearth diameter
(mm)
Hearth height
(mm)
Transformer
secondary electric voltage (V)
Electrode diameter (mm)
Smelting power consumption
HI-6000-DL
Si
6000
4600
1900
104-132
500
13000
HM-6000-DL
Mn3-5
6000
5300
2100
104-132
820
3350
HS-6000-DL
MnSi
6000
5100
2100
104-132
800
4450
HK-6000-DL
Si75
6000
4700
1900
104-132
780
8800
HR-6000-DL
CrSi
6000
4700
1900
104-132
740
5200
HG-6000-DL
Cr4-5
6000
4800
1900
104-132
740
3500
HD-6000-DL
CaC
6000
4800
1900
104-132
760
3000
HM-9000-DL
Mn3-5
9000
6200
2400
101-143
950
3200
HS-9000-DL
MnSi
9000
6000
2300
101-143
920
4500
HK-9000-DL
Si75
9000
5100
2000
101-143
900
8700
HR-9000-DL
CrSi
9000
5100
2000
101-143
880
5100
HG-9000-DL
Cr4-5
9000
5300
2000
101-143
880
3400
HD-9000-DL
CaC
9000
5600
2000
101-143
900
2900
HM-9000-DL
Mn3-5
12500
7100
2800
109-158
1100
HS-9000-DL
MnSi
12500
7000
2700
109-158
1070

No comments: